KIMM and Hanyang University researchers thinned WS₂ by single layers across a six-inch wafer and demonstrated light sensing with memory.

Plasma Etching Sets WS₂ Thickness One Atomic Layer at a Time Across a Six-Inch Wafer

Controlling a two-dimensional semiconductor’s thickness across a wafer is a manufacturing problem as much as a materials science one. Researchers at the Korea Institute of Machinery and Materials (KIMM) and Hanyang University report a plasma etching method that removes tungsten disulfide (WS₂) one atomic layer at a time across a six-inch (15 cm) wafer. They also used the material in an opto-memristor that responds to light and retains information about light pulses.

Nidhi Agarwal
Six-inch wafer scale of WS2 fabricated by KIMM research team, showing SiO₂ substrate, tungsten thin film, and tungsten disulfide wafers with thickness controlled to five, four, three, and two layers
Six-inch WS₂ wafer samples with controlled layer counts, fabricated by the KIMM research team.

Removing layers with brief plasma exposure

The team began with five-layer WS₂ and exposed it to plasma generated from a mixture of three gases. Exposure times ranged from 1 to 4 seconds. Under those conditions, the researchers report removing one atomic layer at a time, producing samples with four, three, and two layers. The thinnest semiconductor film they achieved measured 0.76 nm.

That control addresses a practical obstacle for 2D materials: achieving a chosen thickness consistently over a large area. A process that works on a small sample may produce local variations when applied across a wafer. For devices that depend on atomically thin films, those variations can affect how different regions behave. The reported result is notable because it combines layer-by-layer adjustment with wafer-scale processing, rather than demonstrating thickness control only at isolated points.

The researchers describe the method as the first technology to increase or decrease a semiconductor’s thickness one atomic layer at a time uniformly across a six-inch WS₂ wafer. That is their stated claim. The account does not give a numerical uniformity tolerance, wafer-to-wafer repeatability data, or detailed process conditions beyond the plasma gas mixture and exposure duration, so those measures will matter when assessing process readiness.

The starting surface affects the result

Wafer preparation played a direct role in the final film. The WS₂ was formed from a tungsten film, and the team found that a smoother, more even tungsten surface produced a more uniform WS₂ surface. Where the starting film was rough, some WS₂ layers suffered local damage and the resulting thickness varied.

Nidhi Agarwal

This links the etch step to the quality of the material underneath it. Single-layer removal can set the intended layer count, but it cannot erase defects already introduced by an uneven starting surface. In practice, this means thickness control depends on both the etch process and the condition of the tungsten film. The researchers used electron microscopy and other analyses to examine the material at surface and atomic-layer scales.

The process therefore offers a way to adjust thickness, while the substrate and precursor film remain part of the control problem. For engineering teams evaluating 2D semiconductor fabrication, the surface finding is a reminder to treat incoming film quality as a process variable alongside plasma exposure. Further data on thickness variation across the wafer would help show how tightly the method controls that interaction.

A light sensor that retains pulse history

The researchers used four-layer WS₂ to make an opto-memristor, a device that combines light response with memory behaviour. Its electrical state can reflect prior light input, allowing it to sense pulses and retain a record of them. The four-layer device distinguished all 16 combinations of four on/off light pulses, corresponding to a four-bit input, and stored those combinations in different states.

That demonstration connects the materials process to a device function: changing the number of atomic layers may provide a way to tune memory behaviour. The report does not specify how each layer count changes the device’s response, or provide operating voltages, switching times, endurance, or retention measurements. Those details would be needed to compare the device with other memory elements or assess its suitability for a particular circuit.

The team also evaluated the device using reservoir computing, a computing approach that uses a system’s changing internal states to help classify signals. In the reported analysis, the model classified five types of signal waveforms with an average accuracy of 95.8 per cent. The result indicates that the device’s response to light pulses could support signal classification, though the available account does not describe the dataset, test conditions, or comparison baseline. The accuracy figure should be read within those limits.

What the result establishes

The work brings together two demonstrations: layer-by-layer thickness adjustment over a six-inch WS₂ wafer, and a four-layer device that senses light while retaining pulse-dependent states. The first addresses the challenge of controlling an atomically thin material at useful wafer scale. The second shows one possible function that thickness-controlled WS₂ can support.

For process development, the next useful evidence would include quantified wafer uniformity, repeatability across fabrication runs, and fuller descriptions of the etch conditions and device performance. For the computing demonstration, details of waveform generation and evaluation would clarify how broadly the reported classification result applies. For now, the central engineering takeaway is that plasma exposure can be used to select WS₂ layer count at wafer scale, while starting-surface quality remains a key influence on the resulting film.

Source: Nidhi Agarwal · www.electronicsforu.com

Filed alongside