Hydrogen Bubble Size Shapes Voltage Loss in Alkaline Electrolysers
A 3D model links bubble footprint to voltage losses in alkaline electrolysis, with increases exceeding 50% in some simulated cases.

A hydrogen bubble’s contact area with an electrolyser electrode can matter more to energy loss than the gas bubble’s presence alone. A three-dimensional simulation developed by researchers at Cornell University and City University of Hong Kong points to a critical bubble size: once a bubble grows beyond it, the extra voltage needed for electrolysis can rise sharply.

The finding directs attention to a local feature of electrode operation: the patch of surface masked by an attached bubble. In an alkaline water electrolyser, hydrogen forms at the electrode and bubbles can remain in contact with it as they grow. The researchers modelled a single bubble to isolate how that contact affects performance, rather than trying to infer an individual bubble’s effect from a field of bubbles.

Electrode coverage drives the added voltage
The team found that the area occupied by the bubble on the electrode was the dominant source of bubble-related energy loss in the model. A bubble covering more of the active surface leaves less electrode area available for the electrochemical reaction. The cell then needs additional voltage to sustain hydrogen production under the modelled conditions.

That makes bubble size a practical design variable. Electrode geometry and surface features influence how bubbles attach, spread and detach; understanding the voltage penalty associated with a bubble’s footprint could help researchers compare those design choices. The work does not establish a preferred electrode configuration, but it offers a way to evaluate how an individual bubble’s dimensions relate to the extra voltage requirement.

Lenan Zhang of Cornell University and Weihong Li of City University of Hong Kong led the research. Zhang described the challenge of examining bubbles individually: “It’s really challenging to isolate the impact of bubbles on each individual scale.” A model that can represent a single bubble gives researchers a controlled setting for examining those effects before adding the complexity of multiple bubbles and their interactions.

A threshold ratio offers a design metric
The researchers also developed a ratio comparing the bubble’s separation radius with its critical radius. In the simulations, the voltage increment caused by a single bubble stayed within 3 percent when that ratio was below one. In some other simulated cases, the voltage increase was more than 50 percent relative to the case without a bubble.

Those results suggest that the effect is not captured by simply asking whether a bubble is present. Its size relative to the critical scale matters. The ratio gives future modelling work a way to sort conditions where bubble-induced voltage changes remain limited from those where they may become much larger.

The reported values come from simulations of one bubble, so they describe the modelled cases rather than a measured performance guarantee for commercial electrolysers. Actual systems involve many bubbles, evolving operating conditions and electrode surfaces with specific geometries. The next step is to determine how those factors alter the single-bubble relationship.
Fast simulations could support broader comparisons
Cornell says the model runs 1,000 times faster than other similar models performing equivalent calculations. That computational speed could make it practical to run larger sets of simulations across different electrode types. Such comparisons could help identify which surface designs merit more detailed experimental study.
For electrolyser development, faster modelling is useful when it narrows the range of designs that need to be tested. Bubble behaviour affects the relationship between electrical input and hydrogen output, so reducing the extra voltage associated with bubbles could improve energy efficiency. The simulation provides a mechanism-focused tool for investigating that opportunity; it does not yet show that a particular electrode has achieved such a reduction in a physical system.
The researchers identify modelling interactions among bubbles as a next task, along with combining the model with computational optimization and additive manufacturing. Multi-bubble modelling will matter because neighbouring bubbles may alter available electrode area and change how bubbles grow or leave the surface. Experimental evidence will also be needed to establish how well the simulated single-bubble effects carry over to operating electrolysers.
Relevance to hydrogen production targets
India’s National Green Hydrogen Mission targets annual green hydrogen production capacity of 5 million tonnes by 2030. Electrolysers use electricity to split water, making the voltage required for that process a direct efficiency consideration. A better account of bubble-related losses could inform electrode research aimed at limiting the electrical overhead of hydrogen production.
The immediate engineering value lies in a clearer link between bubble footprint and voltage penalty, backed by a model that can be run quickly. The key question now is how that single-bubble result changes when researchers include interacting bubbles and compare predictions with experimental measurements.
AMD Venice Uses 2.5D Packaging to Feed More Bandwidth Into EPYC Zen 6
CNC Controller Board Design: Interfaces, PCB Specs and Assembly Testing
Stratasys and Nano Dimension End $42.5 Million Markforged Sale Agreement